Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry
Digital.png
  • Load image into Gallery viewer, Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry
  • Load image into Gallery viewer, Digital.png

Standard Test Method for Transition Temperatures and Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry

Regular price
£68.00
Sale price
£68.00
Regular price
£61.20
Sold out
Unit price
per 

1.   Scope*

This test method covers determination of transition temperatures and enthalpies of fusion and crystallization of polymers by differential scanning calorimetry.

NOTE 1— True heats of fusion are to be determined in conjunction with structure investigation, and frequently, specialized crystallization techniques are needed.