Specification and qualification of welding procedures for production welding of steel and nickel-base castings

Regular price
£126.00
Sale price
£126.00
Regular price
£113.40
Sold out
Unit price
per 

1 Scope

This document specifies how a welding procedure specification (WPS) for production welding of steel castings is qualified. Tests are intended to be carried out in accordance with this document, unless additional tests are specified by the purchaser or by agreement between the contracting parties.

This document defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of essential variables.

This document applies to the arc welding of steel castings. The principles of this document can be applied to other fusion welding processes subject to agreement between the contracting parties.