Specification and qualification of welding procedures for metallic materials. Qualification based on tested welding consumables

Specification and qualification of welding procedures for metallic materials. Qualification based on tested welding consumables

Regular price
£166.00
Sale price
£166.00
Regular price
£83.00
Sold out
Unit price
per 

1   Scope

This document specifies how a welding procedure can be qualified by using tested welding consumable data. It expands on the requirements given in ISO 15607.
In addition, it gives the range of qualification.
This document is applicable to the welding processes according to Table 1.
Table 1 — Applicable welding processes
Process
number
according to ISO 4063:2009
Welding process
111 Manual metal arc welding (metal arc welding with covered electrode)
114 Self-shielded tubular cored arc welding
121 Submerged arc welding with solid wire electrode
131 MIG welding with solid wire electrode
132 MIG welding with flux-cored electrode
133 MIG welding with metal cored electrode
135 MAG welding with solid wire electrode
136 MAG welding with flux cored electrode
138 MAG welding with metal cored electrode
141 TIG welding with solid filler material (wire/rod)
15 Plasma arc welding
311 Oxyacetylene welding
Application of this document is limited to parent material groups 1.1, 8.1, 21, 22.1 and 22.2 in accordance with ISO/TR 15608, which produce acceptable microstructures and properties in the heat-affected zone which do not deteriorate significantly in service.
This document is limited to:
  1. — parent material thicknesses t ≤ 40 mm (groups 1.1 and 8.1) and t ≤ 20 mm (groups 21, 22.1 and 22.2);
  2. — fillet welds with throat thickness a ≥ 1 mm.
This document is not applicable when any of the following is specified for the welded joint:
  1. a) hardness;
  2. b) impact properties;
  3. c) preheating;
  4. d) controlled heat input;
  5. e) interpass temperature;
  6. f) post-weld heat treatment.
The use of this document can also be restricted by an application standard, specification or other documents.