1   Scope

This Technical Specification provides guidance for the minimum content of welding procedure specifications for the following welding processes:
  • — hot gas welding: round nozzle, high speed nozzle, wedge;
  • — extrusion welding;
  • — heated tool welding: butt, socket, wedge;
  • — solvent welding: socket;
  • — electrofusion welding: socket, saddle.
This Technical Specification applies to the welding of the following products and semi-finished products made of thermoplastic materials:
  • — sheet;
  • — pipe;
  • — fittings;
  • — lining membrane.