1 Scope
The document specifies a method for undertaking uniaxial constant load testing of
the susceptibility of a metal, or an alloy, to stress corrosion cracking (SCC) in
high-purity water environments at high temperature (above the boiling point of water
at normal pressures) and pressure. The test method is particularly applicable to simulated
primary water environments of light water reactors (LWRs).
The test method enables assessment of the relative resistance to SCC of a material
in different environments and the comparative resistance of different materials (using
the same environment, specimen dimensions and loading).
The terms “metal” and “alloy”, as used in the document, include weld metals and weld
heat affected zones.