Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water

Regular price
£232.00
Sale price
£232.00
Regular price
£116.00
Sold out
Unit price
per 

1   Scope

This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.
The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.